Hai,

There is any corrosion resistance limitation please let me know if any standard acceptance criteria? This pipes are API 5L Gr.B ERW 450 mm Pre insulated pipes. Photos attached here.








REGARDS,

G.SRIRAM.

Dream,Dream,Dream Dream transforms in to thoughts.And thoughts result in action
 
 http://files.engineering.com/getfile.aspx?folder=bda21f41-d057-4ad6-a2b7-ddaeeebdc842&file=IMG_6070.JPG
Nice looking pipes with surface rust blooming - what's wrong with them?

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
Unless it's got pitting or imperfections that exceed 12.5% of the wall thickness, it meets the 5L criteria.
 
As LittleInch said, "What's wrong with them?" Typical rust bloom from outside storage.
 