Apr 28, 2010 #1 Makun Mechanical Joined Jul 20, 2009 Messages 57 Location AR Hi, I was wondering if is possible to make an API 579 S4 for a whole Pipeline. I've a situation of one Pipeline wich required thickness is 1mm below the average measured. Is possible make this kind of analysis? What another choice do I have?
Hi, I was wondering if is possible to make an API 579 S4 for a whole Pipeline. I've a situation of one Pipeline wich required thickness is 1mm below the average measured. Is possible make this kind of analysis? What another choice do I have?
Sep 7, 2010 1 #2 integridadmecanica Mechanical Joined May 1, 2010 Messages 7 Location AR Dear Maku, Yes you can perform a Fitness For Service for general metal loss by API 579. Other choice is ASME B31G. Kind regards Fernando Upvote 0 Downvote