enginesrus
Mechanical
I have some specific questions about some of the marine engines.
Follow along with the video below to see how to install our site as a web app on your home screen.
Note: This feature may not be available in some browsers.
enginesrus said:It difficult to believe that it works that well, its not a low stress area like a cast iron water jacket crack.
I was mainly just commenting on what you posted. I would like to see LARGE cast iron engine blocks or frames, repaired, that were destroyed by pistons and rods exiting. I would think that if most of the pieces from a block where very small and very numerous, that pinning would be out of the question.catserveng said:You earlier asked about crankcase repairs, now you're asking about crankshaft repairs, might be helpful if you could be clear about what you're asking about and what your concerns are.
There are in place repair procedures for crankshaft bearing surfaces, not aware of any currently acceptable field repairs for a crankshaft with cracks going beyond the journal surface.
MikeL.