Friends,
Our technology group asked us to identify an excahnger which can be used to test four types of twisted tube type inserts (turbulators). We don't really have a non-critical exchanger to do this, but are willing to make accomidation for them. My previous locations had standards specifically prohibiting the use of inserts, not sure why, but for this reason I have no experience. My current location does not have any standards addressing the use of these devices.
Can anyone with experience give me some feedback on the success and problems associated with these devices. Our cooling water is very very dirty (muddy and biological solids). We we worry about fouling, maintenance (removal) etc. Any feedback could be useful. These are the models we are asked to try and the application description we got:
SPIRELF – suitable for long service time and velocities greater than 1.5 m/s
TURBOTAL – better performance than the one above but limited service time and applicable with velocities below 2 m/s
FIXOTAL – convenient for wall temperature dependent type of fouling (it doubles effectively the fluid velocity)
Hi-Tran of CAL GAVIN (good only for specified range of operating conditions), Scaling is potentially a big problem for these inserts.
best wishes,
sshep
Our technology group asked us to identify an excahnger which can be used to test four types of twisted tube type inserts (turbulators). We don't really have a non-critical exchanger to do this, but are willing to make accomidation for them. My previous locations had standards specifically prohibiting the use of inserts, not sure why, but for this reason I have no experience. My current location does not have any standards addressing the use of these devices.
Can anyone with experience give me some feedback on the success and problems associated with these devices. Our cooling water is very very dirty (muddy and biological solids). We we worry about fouling, maintenance (removal) etc. Any feedback could be useful. These are the models we are asked to try and the application description we got:
SPIRELF – suitable for long service time and velocities greater than 1.5 m/s
TURBOTAL – better performance than the one above but limited service time and applicable with velocities below 2 m/s
FIXOTAL – convenient for wall temperature dependent type of fouling (it doubles effectively the fluid velocity)
Hi-Tran of CAL GAVIN (good only for specified range of operating conditions), Scaling is potentially a big problem for these inserts.
best wishes,
sshep