Good Afternoon,

Could anyone advise me on an anti - static hose (10mm ID) which gives good flexibility & elasticity i.e. Silicone? Temperatures of 0 up to 70°C. It needs to fit onto hosetails.

Any help much appreciated.

Thanks
 
Interesting, I have never heard the term hosetail before. It must be a British term. In the U.S. they are called barbed fittings. With the information provided almost any type of hose with antistatic additives would work. The important information you neglected to provide is the pressure and the fluid service.
 
Be sure what you want, do you want it conductive, or to dissipate static? Those are two different things.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 