I am looking for some help. Here are the conditions.
I start with sa-182 (sometimes 479) 304ss or 316ss bar.
-drill and ream a 1/4" hole through.
-insert precision ground rod into hole with 0.0000" to 0.0001" total clearance. requires moderate hammer hits to insert.
-finish machine surface perpendicular to rod/hole
-remove pin in direction away from machined surface with slide hammer
When rod is removed I am looking to achieve a burr free very sharp hole edge in addition to no galling on the way in or out. Ive used 304 to 304 and graphite powder and had slight to moderate gallin on the i.d. of the hole and rod.
-Suggestion for rod material that i can use to both avoid galling under this condition yet maintain like machinability so i have a burr free..very sharp hole left when i pull the rod out.
-lubrication suggestion for this condition?
I appreciate any help..thank you..
I start with sa-182 (sometimes 479) 304ss or 316ss bar.
-drill and ream a 1/4" hole through.
-insert precision ground rod into hole with 0.0000" to 0.0001" total clearance. requires moderate hammer hits to insert.
-finish machine surface perpendicular to rod/hole
-remove pin in direction away from machined surface with slide hammer
When rod is removed I am looking to achieve a burr free very sharp hole edge in addition to no galling on the way in or out. Ive used 304 to 304 and graphite powder and had slight to moderate gallin on the i.d. of the hole and rod.
-Suggestion for rod material that i can use to both avoid galling under this condition yet maintain like machinability so i have a burr free..very sharp hole left when i pull the rod out.
-lubrication suggestion for this condition?
I appreciate any help..thank you..