Dimensioning a forging with a size dimension ie: "6.0 MIN".
Per 2.5 I interpret the size limit to be 6.0 to infinity.
There are others that say the drawing tolerance block dictates the maximum size tolerance with the dimension decimal places.
As I replied in your other thread (by the way I suggest you redflag the other thread and ask management to delete it.)
You are correct, your colleagues are at best ignorant.
ASME Y14.5M-1994 section 2.5 Single Limits
...Single limits are used where the intent will be clear, and the unspecified limit can be zero or approach infinity and will not result in a condition detrimental to the design.
(Sorry, I'm in a bit of a bad mood today and my gladly suffering fools threshold is a little low.)
You are correct, unless dimensions on your forging specify something like "MIN full thread, MAX drill depth".