Hello Friends,
We are designing Propane Mounded Storage Tank for Water Capacity of 119,000 Liters. Here are the following details with the SS.
Working Pressure - 12 kg/cm^2 (171 psi)
Design Pressure - 21.356 kg/cm^2 (304 psi)
Corrosion Allowance - 1.5 mm (Is it fair to have 1.5 mm (0.059") or should we go for 3 mm (0.11")as it is ?)
Temperature - (-)42 deg C (-41.11 deg F) to (+) 55 deg C (131 deg F)
Density of Propane - 0.441 kg/m3 (0.02753lb/ft3)
for more details pls see the attachment
My query is, how come the nozzle is failing for 300# and passing for 150# ? Nozzle is failing at MAWP. MAWP is 22.33 kg/cm2 (317psi)
Your kind response will be highly appreciated.
Regards
We are designing Propane Mounded Storage Tank for Water Capacity of 119,000 Liters. Here are the following details with the SS.
Working Pressure - 12 kg/cm^2 (171 psi)
Design Pressure - 21.356 kg/cm^2 (304 psi)
Corrosion Allowance - 1.5 mm (Is it fair to have 1.5 mm (0.059") or should we go for 3 mm (0.11")as it is ?)
Temperature - (-)42 deg C (-41.11 deg F) to (+) 55 deg C (131 deg F)
Density of Propane - 0.441 kg/m3 (0.02753lb/ft3)
for more details pls see the attachment
My query is, how come the nozzle is failing for 300# and passing for 150# ? Nozzle is failing at MAWP. MAWP is 22.33 kg/cm2 (317psi)
Your kind response will be highly appreciated.
Regards