I need to shear test samples from a heat treat load.
Requirement is Inspection level S3, AQL 1.5 non-conforming.
If the customer's order is 2 parts, it seems I need to make (10). (2)to ship and (8) to shear test. - right?

What if the order is for (1)pin? There is no table listing for (1) piece. WHY does the table start at (2)?
 