I'm want to know the difference between a Flange ANSI 16.5 vs ANSI 16.36.

Is it possible to use a flange 16.5 instead a Flange 16.36.

I'll appreciate your help,

Thanks,
 
Replies continue below

Recommended for you

ASME 16.5 is for regular pipe flanges and ASME 16.36 is for Orifice Flanges.