Now we are confronted with a fine-particle runing out problem with our activated carbon filter(ACF) in our UPW plant.
The plant was started 2 months ago. We took SDI sampling outlet ACF recently and were suprised to find that a grayish color on the membrane. And we found similar color downstream ACF, even after RO.
We tested our AC, the specifications were listed below:
coconut shell type
Iodine value: more than 1000
Hardness: more than 95%
size: 14-40mesh US
all these data met our requirements.
And the tank design is no problem, we used for a lot projects.
we use downflow operating mode.
But the fine particle is still running out ACF.
Anybody can help?
thank a lot for your experience and suggestions.
Sunbird
from China, Shanghai.
Now we are confronted with a fine-particle runing out problem with our activated carbon filter(ACF) in our UPW plant.
The plant was started 2 months ago. We took SDI sampling outlet ACF recently and were suprised to find that a grayish color on the membrane. And we found similar color downstream ACF, even after RO.
We tested our AC, the specifications were listed below:
coconut shell type
Iodine value: more than 1000
Hardness: more than 95%
size: 14-40mesh US
all these data met our requirements.
And the tank design is no problem, we used for a lot projects.
we use downflow operating mode.
But the fine particle is still running out ACF.
Anybody can help?
thank a lot for your experience and suggestions.
Sunbird