I'm used working according to EN/ISO standards for welder and procedure qualifications, however I'm trying to have a better understanding of the ASME IX philosophy.
Next question is a theoretical example, purely for my better understanding.
A V-groove butt weld, welded on a 1/2" plate, first two passes using GTAW (deposited thickness: 3/16"), fill and cap using gas shielded FCAW (deposited thickness: 3/8")
There are impact requirements.
I have two different answers for the range of validity of the base metal thicknesses, would someone please check if one of those is correct, or perhaps if there is a third possibility?
A
---
For GTAW: plate thickness from 1/2" (according to QW-403.6) to 1" (according to QW-451.1), max. deposited thickness is 3/8"
For FCAW: plate thickness from 1/2" (according to QW-403.6) to 1" (according to QW-451.1), max. deposited thickness is 3/4"
B
---
For GTAW: plate thickness from 3/16" (according to QW-200.4(a) and QW-451.1) to 1" (according to QW-451.1), max. deposited thickness is 3/8"
For FCAW: plate thickness from 3/16" (according to QW-200.4(a) and QW-451.1) to 1" (according to QW-451.1), max. deposited thickness is 3/4"
It would help tremendously not only to reply with "option A" or "option B", but additionally also to explain why. The train of thoughts is more important than the correct answer here.
Thanks in advance...
Next question is a theoretical example, purely for my better understanding.
A V-groove butt weld, welded on a 1/2" plate, first two passes using GTAW (deposited thickness: 3/16"), fill and cap using gas shielded FCAW (deposited thickness: 3/8")
There are impact requirements.
I have two different answers for the range of validity of the base metal thicknesses, would someone please check if one of those is correct, or perhaps if there is a third possibility?
A
---
For GTAW: plate thickness from 1/2" (according to QW-403.6) to 1" (according to QW-451.1), max. deposited thickness is 3/8"
For FCAW: plate thickness from 1/2" (according to QW-403.6) to 1" (according to QW-451.1), max. deposited thickness is 3/4"
B
---
For GTAW: plate thickness from 3/16" (according to QW-200.4(a) and QW-451.1) to 1" (according to QW-451.1), max. deposited thickness is 3/8"
For FCAW: plate thickness from 3/16" (according to QW-200.4(a) and QW-451.1) to 1" (according to QW-451.1), max. deposited thickness is 3/4"
It would help tremendously not only to reply with "option A" or "option B", but additionally also to explain why. The train of thoughts is more important than the correct answer here.
Thanks in advance...