Ok, this may be a silly question but what is the difference between 8625D and 8625C?? Is it just colour...

thanks
Mike
 
Replies continue below

Recommended for you

Stating "Class 2" would define a colored anodize. The "C" and "D" refer to the revision of the stadard for MIL-A-8625.

[green]"I think there is a world market for maybe five computers."[/green]
Thomas Watson, chairman of IBM, 1943.
Have you read faq731-376 to make the best use of Eng-Tips Forums?
 
Also note that 8625B & 8625C are obsolete revisions.
The current version is MIL-A-8625F and is a free download at ASSIST-Quick Search:

Revision history:

MIL-A-8625F
10 September 1993, Amended 15-SEP-2003
SUPERSEDING
MIL-A-8625E
25 April 1988

Which had superseded
MIL-A-8625D
30 June 1985

Which had superseded
MIL-A-8625C
15 January 1968

Anodize Class per MIL-A-8625F: Class 1 is non-dyed (natural), Class 2 is dyed.
You must also specify Type: Type I for chromic, Type II for conventional, Type III for hard.