I have a Dassault Aviation general specification that references BF4/BF5 anodizing treatment. I've never heard of this. Its not mentioned in MIL-A-8625 and web searches are not giving me any information.
Has anyone encountered this?
Does this have a MIL-A-8625 equivalent?
 
As Dassault is a French company, it may be a type of anodizing defined within the French spec. NF A-91-450 (Décembre 1981) Traitement de surface des Métaux – Anodisation de l’alu et de ses alliages. Spécifications générales.
[“Anodizing of aluminum and its alloys – general specifications for anodic oxide coatings on aluminum.”]

Maybe contact Dassault directly
or the European Anodizing Association (EURAS) [I cannot locate, it may have morphed into the Association for European Surface Treatment on Aluminium , but the link I found seems dead].

If I had to guess, judging from the age of the spec. and its aircraft use, it might be chromic acid anodizing (MIL-A-8625F Type I, IB or IC)
However, a wrong guess could be very expensive so here are some other places to try:
The European Aluminium Association Pechiney Aluminium
Their anodized aluminum sales manager (for export) is
Marc Jobert
Sales manager - Export
33 04 76 97 21 00
33 04 76 97 21 05
bandoxal_bandoxal@pechiney.com
 
The Association for European Surface Treatment on Aluminium is at However, their website only mentions sulfuric acid anodizing and painting as finishes for aluminum, not chromic acid anodizing.
 
The French anodizing specification AFNOR NF A91-450 is available for $46US (hard copy, 11 pages) from Global Engineering:
 
jdsewell

BF4 and BF5 are both oxalo-chromic anodisation operations (with slighly varying compositions and bath temperatures) They are described in Dassault spec. CR 0.4.2.27. Four further companies in France are approved by Dassault for this process, aside from the first link IRstuff provided you.
 