Hi everybody !

A quick question :
My supplier of salted water filters has put the galvanic anodes in the top part of the filters. The entrance of the filters is by the side approximatively at 4/5 of the height of the filters, so the anodes won't be in the water, except during the washing (the flow is then countercurrent).

I believe the anode have to be into the liquid to be useful, will this design work ?

Thanks !
Daniel
 
Maybe he has them upside down?
Yes, the anodes need to be submerged to help.

= = = = = = = = = = = = = = = = = = = =