Dear ALL,
I am working on a tank with design height of 18.4 m and with a liquid having S.G of 1.5. Product of design height and S.G came out to be greater than 23, so i had to perform elastic analysis in finding annular plate thickness.
Now one option is to use find out thickness using ANSYS, but there is a procuder given in BOB LONG'S book. I have prepared an excel sheet using those formulas. Has any one gone through that example in bob long's book??
After preparing the sheet i found out basically you make sure that
1) fatigue stress comes out to be less than 75000 lbs/in2.
2) at the same time you have make sure that θs is equal but with opposite sign to θc and θb is zero
i am confused at one thing that for a given thickness say 8 mm by iteration i found out that 480.55 mm is the width where all conditions are satisfied, but when i increase the width to 700 mm so that the api 650 minimum width requirement of 600 mm is met, fatigue stress becomes greater than 75000 lbs/in2.
so i found out that at 14 mm thickness i can use annular plate of 659.013 mm and the same time fatigue stress is within limit.i cannot go for lower thickness otherwise 600 mm minimum requirement of api 650 and fatigue stress less than 75000 cannot be met.Even at the end of the example in bob long it says that API 650 minimum width of 600 mm is conservative
please share you opinion.
Regards,
Inam
I am working on a tank with design height of 18.4 m and with a liquid having S.G of 1.5. Product of design height and S.G came out to be greater than 23, so i had to perform elastic analysis in finding annular plate thickness.
Now one option is to use find out thickness using ANSYS, but there is a procuder given in BOB LONG'S book. I have prepared an excel sheet using those formulas. Has any one gone through that example in bob long's book??
After preparing the sheet i found out basically you make sure that
1) fatigue stress comes out to be less than 75000 lbs/in2.
2) at the same time you have make sure that θs is equal but with opposite sign to θc and θb is zero
i am confused at one thing that for a given thickness say 8 mm by iteration i found out that 480.55 mm is the width where all conditions are satisfied, but when i increase the width to 700 mm so that the api 650 minimum width requirement of 600 mm is met, fatigue stress becomes greater than 75000 lbs/in2.
so i found out that at 14 mm thickness i can use annular plate of 659.013 mm and the same time fatigue stress is within limit.i cannot go for lower thickness otherwise 600 mm minimum requirement of api 650 and fatigue stress less than 75000 cannot be met.Even at the end of the example in bob long it says that API 650 minimum width of 600 mm is conservative
please share you opinion.
Regards,