The min annealing temp is usually in the applicable material specification.
Since SA-276 doesn't say then go to producers literature.
We would adjust the temp based on actual C content, but 1550F is a good starting point.
= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube