Hello, I am having some thin parts 1.25" wide x 2.50" long machined from .125" thick PTFE sheet. Problem is the sheets come in with a curl to them so the parts don't lie too flat on the mill. Is there a way to anneal the sheets to get the curl out? Thanks!