Can anyone tell me where I can get curves showing the effect on Room Temperature UTS & Proof strength of 2014-T651 Aluminium alloy, after being subjected to a particular temperature-time history? I am coating some parts with Rilsan nylon at 310C for 15 minutes. ESDU data sheets only go up to 250C. MIL-HDBK-5 only has room temp. data for 2024-T3.
 
Replies continue below

Recommended for you

This type of data may not exist in the public domain. I would recommend finding a copy of the following reference to see if it has what you need:

Properties of Aluminum Alloys: Tensile, Creep and Fatigue Data at High and Low Temperatures


If it isn't in this book, then try Alcoa or Alcan. They may have unpublished data on this.
 