I need an anneal heat treat cycle for AISI 1215 and what magnetic properties will this give me?
 
I recommend annealing in vacuum or dry hydrogen atmosphere at 1650degF for 1 hour minimum (add more time if your material is thick).

This will optimize the magnetic properties for the material. I can't give you the exact properties because that will vary from batch to batch.

For more assistance, a description of your application will help.
 