The note in Table 5-21b specifically states that 'failure pressure only applies to tanks falling under F.1.3 only', which means the tank must be subject to net uplift, in order for failure pressure to exist. Additionally, failure pressure, Pf, as defined in F.6, is only applicable to frangible tanks (API-650 5.10.2.6). So, if the tank diameter is less than 50 ft (or if any other 5.10.2.6 criteria are not met), failure pressure does not exist.