We are installing a new 60 ton overhead crane runway, and the structural engineer recommends a leveling nut be installed beneath the base plate to achieve a level structure and hold the structure in place prior to tightening the anchor bolts and grouting the base plates. I always thought it was best to tension the entire anchor bolt by using blocks of steel to support the leveled structure prior to grouting. The specified 1" dia. anchor bolt material is ASTM F1554, 36ksi. The grout thickness allowance is 2" There are four anchor bolts per base plate. The concrete strength is minimum 4000 psi. The base plate thickness is 1.5"
Please give me some general opinions on this approach. I am aware that the structural engineer's approach is quicker and less costly, but am most interested in the best installation.
Please give me some general opinions on this approach. I am aware that the structural engineer's approach is quicker and less costly, but am most interested in the best installation.