Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JAE on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Amount of tensile machine pressure 1

Status
Not open for further replies.

QAFitz

Materials
Joined
Jul 21, 2005
Messages
121
When a tensile machine is rated at 60,000 lbs or 120,000 lbs, is this the maximum amount of force in lbs the machine can exert ?
We've got a cold one riding on the answer (after work of course). I'm saying yes while my buddy says its based upon the diameter of the sample (i.e., a .505 tensile specimen or a 1/4" bolt).
 
The rating is the maximum force that can be exerted, independent of the sample size.

Sample size is important when considering whether a sample will break at 60,000 lbs. For example, a 0.505 diameter tension specimen can have an ultimate tensile strength of 300,000 psi and break before the limit. A plate specimen with 0.5" thickness and 0.5" width can have an ultimate tensile strength of only 240,000 psi and break before the limit.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Yes, it is gross machine load. Many older machines that were set up for both tension and compression would handle double the rating in comp.
We make 1" x 0.200" wall cold drawn tubing. We usually can't break it with our 60k machine (64k max). So we just record the actual yield and 127ksi as UTS (64,000 lb/area).

= = = = = = = = = = = = = = = = = = = =
Corrosion, every where, all the time.