For dealing with anhydrous ammonia service used in industrial processes, the common material of construction is pressure vessel quality carbon steel plate or piping. The corrosion mechanism is stress corrosion cracking (SCC) at high stress locations (welds) in carbon steel vessels. To avoid SCC, a small amount of water is added to anhydrous ammonia.