Ammonia in Sour Water - CS or Nickel Alloys

Status
Not open for further replies.

Weko

Materials
Feb 28, 2011
48
We are doing a stripping in sour water from FCC that contains water, H2S, Ammonia and phenol.

Since there are no present of chloride and oxidant agent in the Heat & Material Balance. SCC mightly would not hapen.

But I am still consfused in wet ammonia contained in the water. Can any body give some guidance and/or share experience in what materials can be selected?


Before stripping the water, the ammonia is about 3% of mass. While entering the acid gas incerenator it became 60% ammonia, 35% H2S, and the rest is Water. I am thinking Alloyed CS for this line, but still not sure. Or I just go with Nickel Alloy for a safety reason?

Any clue which standard to refer would be helpful.
 
Replies continue below

Recommended for you

OK thx for the clue.. I'll try to look at those standard
 
make treatments to have FCC and consider CCT diagram

- Material & metallurgy engineer -
 