Does anyone know what is the interaction between ammonia and graphite at 800-1200 C under 100-400 torr?
 
Replies continue below

Recommended for you

One thermodynamically possible reaction is ammonia decomposition/methane formation:

4 NH3 + 3 C(gr.) --> 2 N2 + 3 CH4 delta GRxn,298K = -20.6 kcal/mol

As there is an increase in gas volume associated with this rxn., it should be favored by the reduced pressure.
 
There are several CxNyHz compounds, but they don't seem thermodynamically likely, i.e., have delta Gf > 0.

Take a look at the thermo data for 25o in Perry's, 6th Edn. p. 3-149. I don't believe that the increase in T will make a qualitative change. Most of the CxNyHz compounds will thermally decompose, especially with a solid surface to catalyze the reaction.
 
Although ammonia is expected to be at least partly dissociated in the absence of catalysts, books say that with carbon, at read heat, ammonia reacts to give ammonium cyanide.
 
Thank you for the responses so far, what I observed in my reactor systems are, the porous solid graphite turns into powderly carbon compound. This could be that the graphite is slowly decomposing according to reaction:
4 NH3 + 3 C(gr.) --> 2 N2 + 3 CH4 delta GRxn,298K = -20.6 kcal/mol
The graphite as it looses methane it become more porous and began to collapse.

 