Experts,
We have to select the materials of an Amine Unit removing CO2 (Up to 80% removal) from the following gas:
Feed Gas composition:
H2O : 0.18 mol%
CO2 : 16.51 mol%
CO : 2.41 mol%
N2 : 0.30 mol%
H2 : 74.79 mol%
C1 : 5.81 mol%
Total: 100 mol%
Amine Used: Monoethanolamine

What the major damage problems that shall be taken into consideration in this unit regarding the gas composition?

Thank you in advance.
 
Can you first provide what is your findings in this? If anything I feel additional, I will add.
 
Start with API RP 571 and look up amine corrosion and amine stress corrosion cracking, then take it from there.

Steve Jones
Corrosion Management Consultant