Experts,
We have to select the materials of an Amine Unit removing CO2 (Up to 80% removal) from the following gas:
Feed Gas composition:
H2O : 0.18 mol%
CO2 : 16.51 mol%
CO : 2.41 mol%
N2 : 0.30 mol%
H2 : 74.79 mol%
C1 : 5.81 mol%
Total: 100 mol%
Amine Used: Monoethanolamine
What the major damage problems that shall be taken into consideration in this unit regarding the gas composition?
Thank you in advance.
We have to select the materials of an Amine Unit removing CO2 (Up to 80% removal) from the following gas:
Feed Gas composition:
H2O : 0.18 mol%
CO2 : 16.51 mol%
CO : 2.41 mol%
N2 : 0.30 mol%
H2 : 74.79 mol%
C1 : 5.81 mol%
Total: 100 mol%
Amine Used: Monoethanolamine
What the major damage problems that shall be taken into consideration in this unit regarding the gas composition?
Thank you in advance.