How do we get the Appr. Data to work. We set is select it, but it doesn't seem to do anything. Is there a special way to enable it? We used Appr Data 201. Set 201 for 1900hz and 80 duty cycle from the 2000/75 we were using, when we run the program, Freq stays at 2000/75.

Am I missing something obvious?

"I am stuck on Band-Aid brand, 'cause they are stuck on me"
 
Suppose I should let you know what we are struggling with:

5052 Aluminum .250" Thick, we almost have it, unfortunately we do not have a 4.0 Double like the cutting conditions spreadsheet posted here suggests. We think if we could get the Appr. Data to work, it may help.

"I am stuck on Band-Aid brand, 'cause they are stuck on me"
 
What nozzle are you using?

Getting the correct nozzle would be the best course of action.

If I remember correctly you cannot have both approach data and fine edge data enabled so make sure fine edge is not on.
 
We use a regular number 3 nozzle. Speed 34 on fiberlaser 2kw.For me it is very similar than ss. We have a little dross but with our thumb we can remove it.
 