1. We have a new/ used machine LC-2415 alpha II. The operating manual lists the gas choices as 1=oxygen low,2=oxygen med,3=oxygen high,4=nitrogen, 5=shop air. In the cutting contitions that were adjused by the prior owners some have the gas as 7 ?

2. Is there a place I could download the original or possibly a more complete cut condition table ? This a 2kw That we intend to cut 24 ga. to 1/4" stainles with nitrogen assist.

Thanks,
Dan
 
Replies continue below

Recommended for you

I can scan the pages that came with ours, but ours is a 4k machine. Not sure what gas 7 is either.
 
gas 7 on my amada 3015 4kw is hi pressure nitrogen, who pressure is adjusted with a manual regulator on the controller.
 