dho,
Conditions are temperature, concentration, exposure time and other chemicals used in the cleaning solution. In general, you should experience no cracking at temperatures below approximately 150 F. You need to be more forthcoming in divulging just what is in your cleaning solution, the time and temperature of exposure, and the alloy steel and its mechanical properties (based on heat treatment) in order to receive meaningful info.