Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Aluminum

Status
Not open for further replies.

jopalu

Structural
Feb 3, 2006
49
Would anyone please provide me with the Fb, Fv and E values for ASTM B-221/429 Aluminum 6061-T6 or similar? I have Strength of Material books, but, I cannot find those design values.

Thank you ...
 
Replies continue below

Recommended for you

We need to know much more. You may contact the Aluminum Association for their specifications and design guide. The allowable depends on the use of the member, the shape of the member, etc.

Be careful if you do any welding, you must reduce the allowable strength due to the heat from welding. The allowable usually is 0.5Fb within one inch of weld.


Regards,
Lutfi
 
You need to purchase the appropriate code for aluminum for your area. All of the information you need should be in it. For the US, that is probably the Aluminum Design Manual.

Aluminum Design Manual Link

 