Hi Guys
we're designing a new threaded filter can. it threads into a 6060 aluminum cast filter head with trapezoidal threads. I'm wondering if you fellas can give some tips on what would be the best material to use to avoid galling and thread wear. I realize I probably won't eliminate it all together but the part will be repeatedly installed and removed in order to replace the filter inside so I'd like to get the best materials possible to reduce the chances so to speak. Thanks Guys!
we're designing a new threaded filter can. it threads into a 6060 aluminum cast filter head with trapezoidal threads. I'm wondering if you fellas can give some tips on what would be the best material to use to avoid galling and thread wear. I realize I probably won't eliminate it all together but the part will be repeatedly installed and removed in order to replace the filter inside so I'd like to get the best materials possible to reduce the chances so to speak. Thanks Guys!