Could anyone please help me to find the strain hardening exponent for 7075 T6, 6061 T6 and 2014 T6 Aluminum.

Thank you in Advance

NickJK
 
From ASM Handbook, Volume 8, Mechanical Testing and Evaluation, under Component testing,,,,,

7075 T6 monotonic load, n=0.113
6061 data for T651 only, monotonic load, n=0.042
2014 T6 not reported
 
Metengr,

Thank you so very much for the quick response and location of the data.

NickJK
 
Aluminum alloys have a FCC crystal structure and low stacking fault energy, which means that dislocation cross slip is extensive, and therefore they do not significantly strain harden. 2014-T6 will be in the same range as the other two alloys, probably closer to 7075.
 