Feb 24, 2004 #1 yjung Civil/Environmental Joined Dec 29, 2000 Messages 57 Location US what kind of washers, base plate, anchor bolts and so on for the Aluminum structure? Can we use steel anchor bolts, plate, washers etc with aluminum structure? special paint?
what kind of washers, base plate, anchor bolts and so on for the Aluminum structure? Can we use steel anchor bolts, plate, washers etc with aluminum structure? special paint?
Feb 24, 2004 #2 koodi Civil/Environmental Joined Aug 26, 2002 Messages 63 Location US My guess is that the steel will eat through the aluminum--at what rate I have no idea. Maybe someone else will know... Upvote 0 Downvote
My guess is that the steel will eat through the aluminum--at what rate I have no idea. Maybe someone else will know...
Jun 24, 2004 #3 oldhand Civil/Environmental Joined Jun 20, 2003 Messages 11 Location GB This is a well known problem. There are isolator washers and sleeves for connecting aluminium using steel bolts. Upvote 0 Downvote
This is a well known problem. There are isolator washers and sleeves for connecting aluminium using steel bolts.