Hello i recently began working at a company that makes aluminum molds in house to make a large arrangement of parts for use in our machine. Material include PVC, 25% glass filled PE, 30% glass filled, PP, PVDF and a few others.
A lot of the molds run thick parts up to 1/2 with little or no cooling. When the do use cooling, 3/8 lines are used, usually one in one out. We have a coupl of thermolaters that usually run at 100F. Many of the cycles seem lond to me and i wonder it we aren't using the high heat tranfer of alluminum to our advatage. Should i increase line size? layouts? flow from thermolators to increase turbulece? GPM gauges?
I realize that there is not a specific question here. Just hoping to start some kind of discussion.
Another question, i recently got in some test HMWHDPE and UHMW that are injection moldable. They are definatly hard-to-flow(UHMW significantly harder to flow than the HD) materials but they mold. Recently a "buddy" at work told the bosses that my hard to flow material would wear the alluminum mold. I believe that the glass fiber in the RPE and RPP would wear the alluminum more, what do you guys think???
A lot of the molds run thick parts up to 1/2 with little or no cooling. When the do use cooling, 3/8 lines are used, usually one in one out. We have a coupl of thermolaters that usually run at 100F. Many of the cycles seem lond to me and i wonder it we aren't using the high heat tranfer of alluminum to our advatage. Should i increase line size? layouts? flow from thermolators to increase turbulece? GPM gauges?
I realize that there is not a specific question here. Just hoping to start some kind of discussion.
Another question, i recently got in some test HMWHDPE and UHMW that are injection moldable. They are definatly hard-to-flow(UHMW significantly harder to flow than the HD) materials but they mold. Recently a "buddy" at work told the bosses that my hard to flow material would wear the alluminum mold. I believe that the glass fiber in the RPE and RPP would wear the alluminum more, what do you guys think???