Mar 14, 2007 #1 subsearobot Mechanical Joined Jan 19, 2007 Messages 217 Location US Hey Does anyone know where I might find s/n curves for 6061-t6 aluminum?
Mar 14, 2007 1 #2 rb1957 Aerospace Joined Apr 15, 2005 Messages 16,171 Location CA MIL-HDBK 5 ... revJ is available on-line at ... http://assist.daps.dla.mil/quicksearch/ search for document number 5, there are a list of hits (mostly electrical stuff) but it is there ! Upvote 0 Downvote
MIL-HDBK 5 ... revJ is available on-line at ... http://assist.daps.dla.mil/quicksearch/ search for document number 5, there are a list of hits (mostly electrical stuff) but it is there !
Mar 15, 2007 #3 jedward Aerospace Joined Jun 7, 2006 Messages 133 Location US Steinberg (vibration analysis for electronic equipment Wiley) has the curves in 2nd edition but not the third) Figure 12.14 for 6061-t6. Includes some other related materials Upvote 0 Downvote
Steinberg (vibration analysis for electronic equipment Wiley) has the curves in 2nd edition but not the third) Figure 12.14 for 6061-t6. Includes some other related materials