Hey
Does anyone know where I might find s/n curves for 6061-t6 aluminum?

 
Steinberg (vibration analysis for electronic equipment Wiley) has the curves in 2nd edition but not the third) Figure 12.14 for 6061-t6. Includes some other related materials
 