Hello,
We are looking at an application of subsequent forming of aluminum tubes, 3004 alloy, H22 temper. Where can I find elongation data for this material?
The approx geometry will be about 6" diameter x .030 inches thick wall (before forming).
If needed, can we anneal the part before forming to the O condition to provide better elongation for forming? Or can we increase formability some other way?
Thanks.
We are looking at an application of subsequent forming of aluminum tubes, 3004 alloy, H22 temper. Where can I find elongation data for this material?
The approx geometry will be about 6" diameter x .030 inches thick wall (before forming).
If needed, can we anneal the part before forming to the O condition to provide better elongation for forming? Or can we increase formability some other way?