jimrcasper
Structural
I need to embed a 1/2" dia. 6061 aluminum alloy threaded rod in an exist concrete slab. The aluminum is necessary due to high intensity RF fields. The appliedloads are small, the bolts are mainly for maintaining a position. Does anyone know of a epoxy that is used and/or certified for this application. Also will an epoxy seperate the concrete and aluminum a sufficent disatnce to prevent a reaction?