oengineer
Structural
- Apr 25, 2011
- 732
What is the preferred aluminum alloy to be used for handrails in a lift station? 6061-T6 or 6063-T6?
Comments/suggestions are appreciated.
Comments/suggestions are appreciated.
Follow along with the video below to see how to install our site as a web app on your home screen.
Note: This feature may not be available in some browsers.
phamENG said:And don't forget to consider the weld affected zone!
phamENG said:6061-T6 is stronger, but check availability.
dvd said:Another point to make on aluminum - it has no endurance limit, i.e., it will fatigue with enough cycles, even at low stress levels
phamENG said:Who wrote the spec for 6063?
dvd said:The components were drawn down tightly for shipping and the flexing of the flatbed during a cross-country trip resulted in enough cycles to cause fatigue failure.