Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Aluminum Alloy L102

Status
Not open for further replies.

vcz

Mechanical
Aug 23, 2002
6
I am quoting an aerospace fitting that has a material
callout of "Aluminum Alloy L102" in 2.5"Dia. bar. Does
anyone know of a possible source? Is there a similar material that is more availble? Thanks
 
Replies continue below

Recommended for you

Try the designation 2014 instead of L 102. This is a very common alloy for producing parts, especially rivets.
 
I can confirm that L102 is indeed a UK aerospace spec for 2014A T4 and T451 bar and extruded section. Strictly speaking L102 is obsolescent.

It is an update of the older but probably more widely recognised (and even more obsolescent) L64.

[tt]Element Min % Max %
Si 0.5 0.9
Cu 3.9 5.0
Mn 0.4 1.2
Mg 0.2 0.8[/tt]

British Standard L102 has more. It should be available for about £30.
 