Hi,
As far as I know, hard anodizing cannot be perceived as coating. Taking this statement into consideration. I would like to know, from your experiences etc., whether it is expected that the dimensions of an aluminum part change after the anodizing or not.
Although we put the drawing note stating the dimensions apply after treatment. I still want to know if the dimensions and tolerances of the part change after anodizing.
The material is Aluminum 5083 and anodizing is per MIL-A-8625 Type III, Class 1. 0.0015-0.0025 inches thickness.
Best regards
As far as I know, hard anodizing cannot be perceived as coating. Taking this statement into consideration. I would like to know, from your experiences etc., whether it is expected that the dimensions of an aluminum part change after the anodizing or not.
Although we put the drawing note stating the dimensions apply after treatment. I still want to know if the dimensions and tolerances of the part change after anodizing.
The material is Aluminum 5083 and anodizing is per MIL-A-8625 Type III, Class 1. 0.0015-0.0025 inches thickness.
Best regards