I think this question arises from the following very serious situation with Vans Aircraft ... designer/manufacture of homebuilt Acft ... via Kits.
They outsourced kits to a vendor which LASER-cut holes to-size... and compounding the problem... the LASER starter-entry hole was placed at the edge of the nominal Dia hole... then the LASER 'drew' the correct size hole with the LASER... Soooooo each Nominal Dia hole has a small semicircular NOTCH at the edge.
It is unbelievable that the LASER starter hole did not get punched on the inside then disappear as the round hole was cut to Nom Dia. It is also unbelievable that these holes were not all 'pilot/undersized' so they could be line-drilled to size to clean/round-out the ragged holes for riveting. Problem with laser and water jet is the micro-ragged-edge from the cutting processes... VS a 'normal/nominal' round-smooth hole created by a drill-bit.
These holes are inserted into the sheet metal for 'fast-build match-hole tooled kits' that have nominal holes precisely placed for rapid Assy. Cleco-Cleco-Cleco-Cleco... etc to rapidly self-tool/build the sheet metal Assy.... then rivet-rivet-rivet-rivet... etc.
Also, VANS engineering/working specs NEVER covered this particular hole LASER-drilling practice to nominal size... nor appears to have intended the starter notch at the hole edge. LOTS of NON-STANDARD practices at play here. LOTS of unhappy kit builders.
SADLY I know too much about match-hole-tooling Assy method... John Thorp originated this in the 1960s for the Thorp T18... which I learned-about as I 'helped' my dad build his aircraft N455DT 1967-to-1972. AND I also knew about this issue with VANs [vendor] non-standard drilling-practices some months ago.
Apparently the shithashitthefan, now. SAD.
Regards, Wil Taylor
o Trust - But Verify!
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation, Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", HBA forum]