This type of data is not published widely. The closest I have seen is this:
G AlSi9Cu3, Werkstoffnummer 3.2163.01, Rm = 304 MPa, Rp0,2 = 168 MPa, A5 = 4.5%, HB = 103, pG = 383 MPa
GD AlSi9Cu3, Werkatoffnummer 3.2163.05, Rm = 232 MPa, Rp0,2 = 159 MPa, A5 = 2%, HB = 88, pG = 367 MPa
Regards,
Cory