Looking for source of Alumel(94%nickel, 2%aluminum, 3% manganese) and Chromel (90% nickel, 10%chromium) rod and wire.
 
Replies continue below

Recommended for you

Try looking for a supplier of heat treating furnace equipment and supplies. This is industry standard and will be readily available from such a source.

Just nitpicking but it is usually termed Chromel-Alumel.

 
The wire is used for thermocouples and available from Omega and others.
 