Mar 30, 2001 #1 Guest I have to find information on a material used to manufacture a seal. The seal is there for adverse environmental protection (i.e. military wise). "Klingert 400" What is it????
I have to find information on a material used to manufacture a seal. The seal is there for adverse environmental protection (i.e. military wise). "Klingert 400" What is it????
Dec 17, 2002 #2 GFSeals Mechanical Joined Nov 7, 2002 Messages 5 Location US Compressed White Asbestos sheet...obsolete and unavailable. Sorry. Upvote 0 Downvote