Does enybody know something about the AlSi17Cu4Mg material? I would like to know everthing! The most important question is the structural properties! What is the yield stress limit, UTS, Young modulus, Fatigue strength limit etc!

Irwin
 
Replies continue below

Recommended for you

Irwin

Look up Volume 2 of the 9th edition of "Metals Handbook"
published by ASM International (formerly American Society for Metals). Most public libraries have a copy of this book in their reference section. You will note that some of the properties you ask for will vary with temperature and other conditions in the working environment.

Good luck
 