Is there any (affordable) metall available which can withstand a slurry of Aluminumhydrate, Sulphuric acid 98% and water at temp. of 120ºC and 3 - 4 bar?
Im thinking of a reactor of 20 - 25 m3. I know the alternatives like rubber- or glasslined but these have there own problems. I would prefer to skip the lining and do it in a full metall reactor.
 