I am mixing Alodine 600 in 5 gal. container.
My pH requirements are between 1.5-2.0. and a concentration of 2.5-3.5 oz/gal.
How can I raise the pH level without affecting the concentration.
 
Replies continue below

Recommended for you

I want to increase the pH. According to Spec. Sheet adding nitric acid will decrease the pH.
 
Ah, sorry. It contains 40-50% sodium borofluoride so there should be no issue in using sodium hydroxide.
 